'''Making measurements'''
'''Making measurements'''


Opening the SEM images with Irfanview (or any other image viewer with the same possibilities) and drawing squares (the pixel dimensions are shown in the top) as measurements. These squares are one pixel wide compared to the 2 (or even 3) which are default for the annotations in smartSEM.
Opening the SEM images with Irfanview (or any other image viewer with the same possibilities) and drawing squares (the pixel dimensions are shown in the top) as measurements. These squares are one pixel wide compared to the 2 (or even 3) which are default for the annotations in smartSEM.  
 


; Pixel Size (PS)