==Characterisation of etched trenches==
==Characterisation of etched trenches==


The trenches in deep silicon trenches can be characterized in many ways. Being able to compare processes to oneanother requires that a set of common measurements and calculations must be established. Click [[Specific Process Knowledge/Etch/DRIE-Pegasus/TrenchCharacterisation|'''HERE''']] to find more information about the parameters used on the DRIE-Pegasus process development.
The trenches in deep silicon trenches can be characterized in many ways. Being able to compare processes requires that a set of common measurements and calculations must be established. Click [[Specific Process Knowledge/Etch/DRIE-Pegasus/TrenchCharacterisation|'''HERE''']] to find more information about the parameters used on the DRIE-Pegasus process development.