Specific Process Knowledge/Etch/DRIE-Pegasus: Difference between revisions
| Line 57: | Line 57: | ||
! style="background:silver; color:black" | [[Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-3| DRIE-Pegasus 3]] | ! style="background:silver; color:black" | [[Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-3| DRIE-Pegasus 3]] | ||
! style="background:silver; color:black" | [[Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4| DRIE-Pegasus 4]] | ! style="background:silver; color:black" | [[Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4| DRIE-Pegasus 4]] | ||
|- valign="top" | |||
! style="background:lightgrey; color:black" | Manufactured | |||
| style="background:lightgrey; color:black" | 2010 | |||
| style="background:lightgrey; color:black" | 2010 | |||
| style="background:lightgrey; color:black" | ? | |||
| style="background:lightgrey; color:black" | ? | |||
|- valign="top" | |- valign="top" | ||
! style="background:Whitesmoke; color:black" | Serial | ! style="background:Whitesmoke; color:black" | Serial | ||
| Line 63: | Line 69: | ||
| style="background:WhiteSmoke; color:black"| ? | | style="background:WhiteSmoke; color:black"| ? | ||
| style="background:WhiteSmoke; color:black"| ? | | style="background:WhiteSmoke; color:black"| ? | ||
|- valign="top" | |||
! style="background:Whitesmoke; color:black" | Electrode size | |||
! style="background:WhiteSmoke; color:black" | 4" | |||
| style="background:WhiteSmoke; color:black"| 6" | |||
| style="background:WhiteSmoke; color:black"| 6" | |||
| style="background:WhiteSmoke; color:black"| 6" | |||
|- valign="top" | |- valign="top" | ||
! style="background:lightgrey; color:black" | Manufactured | ! style="background:lightgrey; color:black" | Manufactured | ||
| Line 69: | Line 81: | ||
| style="background:lightgrey; color:black" | ? | | style="background:lightgrey; color:black" | ? | ||
| style="background:lightgrey; color:black" | ? | | style="background:lightgrey; color:black" | ? | ||
|- valign="top" | |- valign="top" | ||
! style="background:Whitesmoke; color:black" | Hardware options | ! style="background:Whitesmoke; color:black" | Hardware options | ||
Revision as of 15:57, 25 June 2018
Feedback to this page: click here
The DRIE Pegasus tools at Danchip
In 2010 Danchip acquired DRIE-Pegasus 1 (at the time called DRIE-Pegasus). As a state-of-the-art etch tool with excellent performance and great flexibility, it grew immensely popular and by 2015 it was apparent that we needed yet another tool to cope with the demand. Therefore, in 2016 Pegasus 2 was acquired from a closed-down lab in Morocco and installed next to Pegasus 1.
Then, in 2017 we got our hands on a twin Pegasus system with cassette to cassette vacuum robot at a very reasonable price from a commerciel fab. The twin Pegasus system (will be called Pegasus 3 and 4) will be installed at the old cluster 2 location in cleanroom C1 from August 2018 onwards.
The Bosch process
The DRIE Pegasus tools are state-of-art silicon dry etchers that offer outstanding performance in terms of etch rate, uniformity etc. They use the so-called Bosch process to achieve excellent control of the etched features. Click HERE for more fundamental information of the system. As of 2017, completing the Dry Etch TPT course is mandatory for all new users. On the TPT web page you will find a version of the latest lecture slides - here you will find information as well.
Links to the individual pages for the Pegasi
- DRIE-Pegasus 1
- DRIE-Pegasus 2
- DRIE-Pegasus 3 - installation in progress
- DRIE-Pegasus 4 - installation in progress
Process information
SPTS process notation
Describing a process recipe on the Pegasus may sometimes be difficult because of the great flexibility of the instrument. A compact and precise notation is therefore required for the recipes. Click HERE to find a short description of the official SPTS notation.
Hardware changes
A few hardware modifications have been made on the Pegasus since it was installed in 2010. The changes are listed below.
| DRIE-Pegasus 1 | DRIE-Pegasus 2 | DRIE-Pegasus 3 | DRIE-Pegasus 4 | |
|---|---|---|---|---|
| Manufactured | 2010 | 2010 | ? | ? |
| Serial | MP0636 | MP0641 | ? | ? |
| Electrode size | 4" | 6" | 6" | 6" |
| Manufactured | 2010 | 2010 | ? | ? |
| Hardware options |
|
|
? | ?|- |
General Pegasus information
Wafer bonding
To find information on how to bond wafers or chips to a carrier wafer, click here.
Characterisation of etched trenches
Comparing differences in etched trenches requires a set of common parameters for each trench. Click here to find more information about the parameters used on the DRIE-Pegasus process development.
Material from SPTS