This is a micrometer-screw.
This is a micrometer-screw.



Revision as of 15:17, 21 October 2013

Feedback to this page: [1]


This is a micrometer-screw.

The Thickness measurer in Cleanroom 3

It measures with an accurracy within a few µm. The range is from a few µm up to 5mm. Measure the wafer in the box next to the meter. If this is ok, then other wafers can be measured. There is a calibration device by the DEKTAK. It is calibrated at 750µm.