Revision as of 10:47, 29 August 2008
Deposition of TiW alloy can take place in the Wordentec.
| Sputter deposition (Wordentec) | |
|---|---|
| Batch size |
|
| Pre-clean | RF Ar clean |
| Layer thickness | . |
| Deposition rate | Depending on process parameters, see here. |
This is done by a sputtering process. Process parameters (argon pressure and effect) can be varied, the surface roughness and the deposition rate (see here) and may change with these settings.