Jump to content

Specific Process Knowledge/Etch/KOH Etch/ProcessInfo: Difference between revisions

Kabi (talk | contribs)
Kabi (talk | contribs)
Line 69: Line 69:




(0.85wt%∙X)/(X+1000g)=Y
<math>(0.85wt%X)/(X+1000g)=Y</math>




X=(Y∙1000g)/(0.85wt%-Y)
<math>X=(Y1000g)/(0.85wt%-Y)</math>




Line 80: Line 80:




(0.5wt%∙1.509g/ml∙X)/(X∙1.509g/ml+1000g)=Y
<math>(0.5wt%1.509g/mlX)/(X1.509g/ml+1000g)=Y</math>




X=(Y∙1000g)/(1.509g/ml∙(0.5-Y))
<math>X=(Y1000g)/(1.509g/ml(0.5-Y))</math>