If you use the 50wt% premade solution you can calculate the amount of solution X you need to add 1 liter of water to achieve a concentration of Y wt% by:
If you use the 50wt% premade solution you can calculate the amount of solution X you need to add 1 liter of water to achieve a concentration of Y wt% by:


(0.5∙1.509 g/ml ∙X)/(X∙1,509 g/ml+1000g)=Y
(0.5∙1.509 g/ml ∙X)/(X∙1.509 g/ml+1000g)=Y


X=(Y∙1000g)/(1,509 g/ml∙(0.5-Y))
X=(Y∙1000g)/(1.509 g/ml∙(0.5-Y))


where 1.509 g/ml is the density of a 50wt% solution KOH at 20 °C.  