Specific Process Knowledge/Back-end processing/Polymer Injection Molder: Difference between revisions
No edit summary |
|||
| Line 64: | Line 64: | ||
Topas polymers are supplied by Danchip. All other polymers are purchased by the users themselves. All polymers (and each individual grade of each polymer) must be approved for use at DTU Danchip. If you would like to use a new polymer or a new grade of a certain polymer, please fill out the application form which can be found in LabManager by going to the 'Documents' tab of the 'Info' page for the Polymer Injection Molding machine. You can also click this direct link: [http://labmanager.dtu.dk/view_binary.php?fileId=2857 New_polymer_application.dotx]. | Topas polymers are supplied by Danchip. All other polymers are purchased by the users themselves. All polymers (and each individual grade of each polymer) must be approved for use at DTU Danchip. If you would like to use a new polymer or a new grade of a certain polymer, please fill out the application form which can be found in LabManager by going to the 'Documents' tab of the 'Info' page for the Polymer Injection Molding machine. You can also click this direct link: [http://labmanager.dtu.dk/view_binary.php?fileId=2857 New_polymer_application.dotx]. | ||
When the polymer has been approved you will receive labels which must be used to label your polymer. All polymers left in the injection | When the polymer has been approved you will receive labels which must be used to label your polymer. All polymers left in the injection molding room must be marked with this official DTU Danchip label. '''Polymers not labelled appropriately may be thrown out at any time'''. | ||
The easiest way to get an overview of polymers and processes used on the polymer injection | The easiest way to get an overview of polymers and processes used on the polymer injection molding machine is to go to LabManager and consult the [http://labmanager.dtu.dk/function.php?module=Processlog&view=editlog&machid=278 Process Log for the injection molding machine]. If you would like use a non-Danchip polymer for a test, please contact the owner of the polymer and ask if you can have a sample. A complete list of all polymers in use at DTU Danchip and who owns them can be found in LabManager on the Info page for the polymer injection molding machine on the 'Documents' tab. You can also click this direct link: [http://labmanager.dtu.dk/view_binary.php?fileId=3044 Approved_polymers_list.pdf]. | ||
==Process parameters and optimization== | ==Process parameters and optimization== | ||
There are no standard injection | There are no standard injection molding processes because it varies significantly how users prefer to optimize their process and how they prioritize parameters such as polymer type, replication fidelity, dimensional accuracy, optical properties, residual stress and cycle time. However, browsing through the [http://labmanager.dtu.dk/function.php?module=Processlog&view=editlog&machid=278 Process Log] it's usually not a problem to find a program made for the polymer and tool at hand which can be used as a starting point. | ||
The injection moulding cycle consists of the steps outlined below. Click on each step to get a description of the most important process parameters for each step: | The injection moulding cycle consists of the steps outlined below. Click on each step to get a description of the most important process parameters for each step: | ||
Revision as of 15:22, 9 February 2018
Feedback to this page: click here
Polymer injection molding

The injection molder at Danchip is an Engel Victory Tech 80/45 which is a hydraulic machine with single motor. The machine is also equippmed with a robot which can pick up finished samples and place them on a conveyor belt. See the table below for key capabilities of this machine. The user manual, user APV, technical information and contact information can be found in LabManager:
Polymer injection molding Info on LabManager (Click 'Documents' tab to go to documents).
Equipment performance
The polymer injection molding machine at DTU Danchip is a hydraulic system with the following capabilities:
| Parameter | Value | |
|---|---|---|
| General | Tools |
Flat disc, Disc with Luer connectors, Microscope slide |
| Clamping force |
Up to 450 kN | |
| Processing temperatures | Mold temperature |
~15°C to 160°C (absolute max) |
| Heating cylinder |
Absolute max: 350°C | |
| Molding parameters | Injection speed |
Up to 53 cm3/s |
| Injection pressure |
Up to 2200 bar | |
| Process types |
Constant mold temperature or Variotherm | |
Polymers
At Danchip the following polymers are used routinely:
- Topas 5013L-10
- Topas 8007S-04
- PP
- PMMA
Topas polymers are supplied by Danchip. All other polymers are purchased by the users themselves. All polymers (and each individual grade of each polymer) must be approved for use at DTU Danchip. If you would like to use a new polymer or a new grade of a certain polymer, please fill out the application form which can be found in LabManager by going to the 'Documents' tab of the 'Info' page for the Polymer Injection Molding machine. You can also click this direct link: New_polymer_application.dotx.
When the polymer has been approved you will receive labels which must be used to label your polymer. All polymers left in the injection molding room must be marked with this official DTU Danchip label. Polymers not labelled appropriately may be thrown out at any time.
The easiest way to get an overview of polymers and processes used on the polymer injection molding machine is to go to LabManager and consult the Process Log for the injection molding machine. If you would like use a non-Danchip polymer for a test, please contact the owner of the polymer and ask if you can have a sample. A complete list of all polymers in use at DTU Danchip and who owns them can be found in LabManager on the Info page for the polymer injection molding machine on the 'Documents' tab. You can also click this direct link: Approved_polymers_list.pdf.
Process parameters and optimization
There are no standard injection molding processes because it varies significantly how users prefer to optimize their process and how they prioritize parameters such as polymer type, replication fidelity, dimensional accuracy, optical properties, residual stress and cycle time. However, browsing through the Process Log it's usually not a problem to find a program made for the polymer and tool at hand which can be used as a starting point.
The injection moulding cycle consists of the steps outlined below. Click on each step to get a description of the most important process parameters for each step: