Jump to content

Specific Process Knowledge/Thin film deposition/MVD: Difference between revisions

From LabAdviser
Taran (talk | contribs)
No edit summary
Jmli (talk | contribs)
No edit summary
Line 1: Line 1:
'''Feedback to this page''': '''[mailto:photolith@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/MVD click here]'''
'''Feedback to this page''': '''[mailto:photolith@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/MVD click here]'''


[[Category: Equipment|Thin film MVD]]
[[Category: Equipment|Thin film MVD]]
Line 8: Line 8:
[[image:Mvd.jpg|200x200px|right|thumb|The MVD is located in cleanroom A-1]]
[[image:Mvd.jpg|200x200px|right|thumb|The MVD is located in cleanroom A-1]]


The Applied Microstructures MVD 100 system deposits molecular films on surfaces. These films serve a wide range of purposes ranging from antistiction coatings of nanoimprint lithography stamps to protecting MEMS structures. At Danchip the MVD is an essential tool for nanoimprint lithography, where it is used to create antistiction coatings on the imprint stamps.
The Applied Microstructures MVD 100 system deposits molecular films on surfaces. These films serve a wide range of purposes ranging from antistiction coatings of nanoimprint lithography stamps to protecting MEMS structures. At DTU Nanolab the MVD is an essential tool for nanoimprint lithography, where it is used to create antistiction coatings on the imprint stamps.




'''The user manual, user APV, and contact information can be found in LabManager:'''
'''The user manual, user APV, and contact information can be found in LabManager:'''


[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=199 MVD in LabManager]
[http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=199 MVD in LabManager]


==Process information==
==Process information==

Revision as of 16:11, 25 November 2019

Feedback to this page: click here

The Molecular Vapor Deposition tool

The MVD is located in cleanroom A-1

The Applied Microstructures MVD 100 system deposits molecular films on surfaces. These films serve a wide range of purposes ranging from antistiction coatings of nanoimprint lithography stamps to protecting MEMS structures. At DTU Nanolab the MVD is an essential tool for nanoimprint lithography, where it is used to create antistiction coatings on the imprint stamps.


The user manual, user APV, and contact information can be found in LabManager:

MVD in LabManager

Process information


Equipment performance and process related parameters

Purpose
  • FDTS coating of Si or SiO2 surfaces
  • Indirect O2 plasma treatment
Vapor sources Line
  • 1
  • 2
  • 3
  • 4
Chemical
  • Water
  • FDTS (new source, 2013)
  • FDTS (old source, contaminated line)
  • Available (line probably contaminated, no source heater)
Performance Contact angle

110° (water)

Process parameters Base pressure

20 mTorr

Chamber temperature

35°C

Chamber volume

Approx. 3 liters

Substrates Substrate size

1" to 8"

Smaller samples may be processed if fixed to a carrier

Allowed materials

All cleanroom materials except steel and other ferrous materials

Batch

One sample at a time

Two 4" or 6" wafers may be processed simultaneously using cassettes