The purpose is to measure the thickness of wafers, depths of larger grooves or height of larger mesas.  
There are 2 thickness measurers in the cleanroom, both positioned in cleanroom D-3. The Thickness measurer is for measuring all sorts of samples. The thickness measurer (wafers) is solely for measuring the thickness of wafers or depths of grooves on wafers.  


During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.  
During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.  

Revision as of 08:21, 18 March 2020

Feedback to this page: click here

Thickness measurer

Thickness Measurer. Positioned in cleanroom D-3

There are 2 thickness measurers in the cleanroom, both positioned in cleanroom D-3. The Thickness measurer is for measuring all sorts of samples. The thickness measurer (wafers) is solely for measuring the thickness of wafers or depths of grooves on wafers.

During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.


The user manual, technical information and contact information can be found in LabManager:

Thickness measurer

Quality Control - Recipe Parameters and Limits

Quality Control (QC) for the Thickness measurer

The measured standard thickness is 0.1 mm. The measured result has to be within ± 0.005 mm. The QC is preformed once a year.


Equipment performance and process related parameters

Purpose

Thickness measurer

  • Wafer thickness
  • Depths of larger grooves
  • Heigth of larger mesas

Performance

Thickness resolution

  • < 5 µm

Substrates

Batch size

  • One sample
Substrate materials allowed
  • No restrictions