Specific Process Knowledge/Etch/Wet Silicon Oxide Etch (BHF): Difference between revisions
Appearance
No edit summary |
|||
| Line 12: | Line 12: | ||
SIO etch (BHF with wetting agent) can also be used for etching silicon oxide. This is mainly for etching small holes. If you have wetting problems in BHF try the SIO etch. It is also a good idea to wet the sample in water for a few minutes before etching. | SIO etch (BHF with wetting agent) can also be used for etching silicon oxide. This is mainly for etching small holes. If you have wetting problems in BHF try the SIO etch. It is also a good idea to wet the sample in water for a few minutes before etching. | ||
Wafers with metals or other materials, not allowed in the dedicated oxide etch baths, can be etched | Wafers with metals or other materials, not allowed in the dedicated oxide etch baths, can be etched using a '''plastic''' in Fume hood 1 or 2 in D-3. | ||
'''The user manual for Oxide etch 1: BHF, APV's and contact information can be found in LabManager''' [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=389 by clicking here] | '''The user manual for Oxide etch 1: BHF, APV's and contact information can be found in LabManager''' [http://labmanager.dtu.dk/function.php?module=Machine&view=view&mach=389 by clicking here] | ||