| Line 127: | Line 127: | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
* yes | * yes | ||
* pneumatic dispense for SU-8 resist | * pneumatic dispense for SU-8 resist and EBR solvent | ||
|style="background:WhiteSmoke; color:black"| | |style="background:WhiteSmoke; color:black"| | ||
* Two syringe pumps | * Two syringe pumps | ||