Jump to content

Specific Process Knowledge/Characterization/Probe station: Difference between revisions

From LabAdviser
Rkch (talk | contribs)
Rkch (talk | contribs)
Line 4: Line 4:


==Thickness measurer==
==Thickness measurer==
[[Image:Thicknessmeasurer2007.jpg|thumb|300x300px|Thickness Measurer. Positioned in cleanroom D-3]]
[[Image:probe_station2.jpg|thumb|300x300px|Thickness Measurer. Positioned in serviceroom CX1]]


The purpose is to measure the thickness of wafers, depths of larger grooves or height of larger mesas.  
The purpose is to measure the thickness of wafers, depths of larger grooves or height of larger mesas.  


During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.  
During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.
 
 
'''The user manual, technical information and contact information can be found in LabManager:'''
 
'''[http://www.labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=198 Thickness measurer]'''


==Quality Control - Recipe Parameters and Limits==
==Quality Control - Recipe Parameters and Limits==

Revision as of 11:59, 21 September 2017

Probe Station

Feedback to this page: click here

Thickness measurer

File:Probe station2.jpg
Thickness Measurer. Positioned in serviceroom CX1

The purpose is to measure the thickness of wafers, depths of larger grooves or height of larger mesas.

During a KOH etch it can be helpful to ensure no over-etching by making a thickness measurement during the etching.

Quality Control - Recipe Parameters and Limits

Quality Control (QC) for the Thickness measurer

The measured standard thickness is 0.1 mm. The measured result has to be within ± 0.005 mm. The QC is preformed once a year.


Equipment performance and process related parameters

Purpose

Thickness measurer

  • Wafer thickness
  • Depths of larger grooves
  • Heigth of larger mesas

Performance

Thickness resolution

  • < 5 µm

Substrates

Batch size

  • One sample
Substrate materials allowed
  • No restrictions


The Probe station is a - EPS150Triax - Cascade for I/V measurement, ohmic measurements etc, it has 4 individually adjustable probes, but can be fitted with more. It has several source meters, multi meters and a computer attached.

It can be used from pieces up to 6" wafers

File:Probestation.jpg
Probe station: positioned in Service room CX1

The user manual, technical information and contact information can be found in LabManager:

Probe station