Specific Process Knowledge/Etch/Wet Aluminium Etch: Difference between revisions
Appearance
| Line 64: | Line 64: | ||
|-style="background:WhiteSmoke; color:black" | |-style="background:WhiteSmoke; color:black" | ||
!Process temperature | !Process temperature | ||
| | |50°C | ||
| | |20°C | ||
|- | |- | ||