''NOTE: After depositing 10layers of 10nm each, one on top of eachother, the roughness increased to 0.8nm RMS''
''NOTE: After depositing 10 layers of 10nm each, one on top of each other, the roughness increased to 0.8nm RMS''


Work done by Johneph Sukham ([mailto:johsu@fotonik.dtu.dk?Subject=Thin%20Au%20deposition%20using%20Lesker click to email]) and Radu Malureanu ([mailto:rmal@dtu.dk?Subject=Thin%20Au%20deposition%20using%20Lesker click to email])