Feedback to this page: click here
The Imprinter 02 is a system for bonding. 3 different types of Polymer bonds bonding can be done: PMMA, SU8 and BCB. It not is possible to mechanically align the wafers. It is also possible to process pieces.
The user manual, quality control procedure and results, user APV(s), and contact information can be found in LabManager: Equipment info in LabManager
| Purpose | Bonding |
|
|---|---|---|
| Performance | Alignment accuracy |
|
| Process parameter range | Process Temperature |
|
| Process pressure |
| |
| Piston Force |
| |
| Substrates | Batch size |
|
| Substrate material allowed |
| |
| Material allowed on the substrate |
|