|'''Recommended dice depth'''
|'''Recommended dice depth'''
|Set blade height to 200µm (preferred). This leaves 125µm uncut since blue tape is 75µm.<br> It is possible to cut through the sample.
|Set blade height to 200µm (preferred).<br>This leaves 125µm uncut since blue tape is 75µm.<br> It is possible to cut through the sample.
|Set blade height to 200µm (preferred). This leaves 125µm uncut since blue tape is 75µm.<br> It is possible to cut through the sample.
|Set blade height to 200µm (preferred).<br>This leaves 125µm uncut since blue tape is 75µm.<br> It is possible to cut through the sample.
|-valign="top"
|-valign="top"
|'''Max. sample thickness'''
|'''Max. sample thickness'''