Specific Process Knowledge/Lithography/Coaters: Difference between revisions
Appearance
| Line 692: | Line 692: | ||
'''Training video: [http://podcast.llab.dtu.dk/fileadmin/podcasts/2016/DTUDanchip/1.057_Manual_Spin_Coater-720p.mp4 LabSpin6]''' | '''Training video: [http://podcast.llab.dtu.dk/fileadmin/podcasts/2016/DTUDanchip/1.057_Manual_Spin_Coater-720p.mp4 LabSpin6]''' | ||
Spin curves (LabSpin 6): [[media:AZ5214E_spin_curve.pdf|AZ 5214E]], [[media:Spin_curve_nLoF2020.pdf|AZ nLOF 2020]], [[media:Spin_curve_ZEP520A.pdf|ZEP 520A]], [[media:Spin_curve_Fox-15.pdf|FOX-15]] | Spin curves (LabSpin 6): [[media:AZ5214E_spin_curve.pdf|AZ 5214E]], [[media:Spin_curve_nLoF2020.pdf|AZ nLOF 2020]], [[media:Spin_curve_ZEP520A.pdf|ZEP 520A]], [[media:Spin_curve_Fox-15.pdf|FOX-15]], [[media:AZ5214E_spin_curve.pdf|AZ 4562]] | ||