|Platen temperature [<sup>o</sup>C] | |Platen temperature [<sup>o</sup>C] | ||
| | |20 | ||
|- | |- | ||
|C<sub>4</sub>F<sub>8</sub> flow [sccm] | |C<sub>4</sub>F<sub>8</sub> flow [sccm] | ||