Jump to content

Specific Process Knowledge/Lithography/EBeamLithography: Difference between revisions

Lgpe (talk | contribs)
Lgpe (talk | contribs)
Line 287: Line 287:
|}
|}


<br/>
If the resist is not adhering properly to the substrate, the coating looks like full of pinholes and the edge is not covered, try to remove the resist, dip 30s. in BHF, rinse 5 mins and spin dry, the spin coat again.


<br/>
<br/>