Specific Process Knowledge/Etch/Etching of Bulk Glass: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 9: | Line 9: | ||
* Piranha clean | * Piranha clean | ||
* Bake-out at 250 C (>2.5 hours) | * Bake-out at 250 <sup>o</sup>C (>2.5 hours) | ||
* Plasma ashing | * Plasma ashing | ||
* Sputter-deposit in Alcatel: Power: 550W, Ar-pressure: 10<math>^{-2}</math> mbar (base pressure: 10<math>^{-6}</math> mbar) | * Sputter-deposit in Alcatel: Power: 550W, Ar-pressure: 10<math>^{-2}</math> mbar (base pressure: 10<math>^{-6}</math> mbar) | ||