==Sputtering of Nickel Vanadium== | ==Sputtering of Nickel Vanadium== | ||
Nickel Vanadium may be sputter deposited in either Sputter-system (Lesker) | Nickel Vanadium may be sputter deposited in either Sputter-system (Lesker) | ||
In the chart below you can compare the different deposition equipment. | In the chart below you can compare the different deposition equipment. | ||
Revision as of 10:00, 28 November 2016
Feedback to this page: click here
Sputtering of Nickel Vanadium
Nickel Vanadium may be sputter deposited in either Sputter-system (Lesker)
In the chart below you can compare the different deposition equipment.
| Sputter deposition (Sputter-System Lesker) | |
| General description | Sputter deposition of NiV |
| Pre-clean | RF Ar clean |
| Layer thickness | About 10Å to 5000Å |
| Deposition rate | Depending on process parameters. |
| Batch size |
|
| Allowed substrates |
|
| Allowed materials |
|
| Comment | Sputter target with NiV composition: Ni/V 93/7% |