Line 53: Line 53:
1) Pumping Cube for single TEM specimen holder.
1) Pumping Cube for single TEM specimen holder.
 
 
[[File:IMG_3663.JPG|300px|left|thumb|Location Building 307, Room 111]]<br />
[[File:IMG_3663.JPG|300px|left|thumb|Location Building 314, Prep Room 01]]<br />
 
 
<br clear="all" />
<br clear="all" />
Line 61: Line 61:
[http://www.gatan.com/products/tem-specimen-holders/turbo-pumping-station/ Brochure]
[http://www.gatan.com/products/tem-specimen-holders/turbo-pumping-station/ Brochure]
 
 
[[File:IMG_3677.JPG|250px|left|thumb|Location Building 314, Common area]]<br />
[[File:IMG_3677.JPG|250px|left|thumb|Location Building 314, Prep Room 03]]<br />
 
 
<br clear="all" />
<br clear="all" />
Line 122: Line 122:
[http://www.fischione.com/products/contamination-solutions/model-1020-plasma-cleaner Brochure]
[http://www.fischione.com/products/contamination-solutions/model-1020-plasma-cleaner Brochure]
 
 
[[File:IMG_3682.JPG|250px|left|thumb|Location Building 307, Prep Room 01]].<br />
[[File:IMG_3682.JPG|250px|left|thumb|Location Building 307, Prep Room 03]].<br />
 
 
<br clear="all" />
<br clear="all" />
Line 132: Line 132:
[http://cressington.com/product_208c.html  Brochure]
[http://cressington.com/product_208c.html  Brochure]
 
 
[[File:IMG_3684.JPG|250px|left|thumb|Location Building 314, Prep Room 01]]<br />
[[File:IMG_3684.JPG|250px|left|thumb|Location Building 314, Prep Room 03]]<br />
 
 
<br clear="all" />
2) Quorum Q150T Sputter Coater and Glow discharge
[http://labmanager.dtu.dk/view_binary.php?fileId=3020 Manual]
[[File:xxx.jpg|250px|left|thumb|Location Building 314, Prep Room 03]]<br />
<br clear="all" />
<br clear="all" />
 
 
2) Cressington 208HR Sputter Coater.
<!-- 2) Cressington 208HR Sputter Coater.
 
 
[http://cressington.com/spec_208hr.html  Brochure]
[http://cressington.com/spec_208hr.html  Brochure]
Line 151: Line 159:
[[File:IMG_3687.JPG|250px|left|thumb|Location Building 314, Prep Room 01]]<br />
[[File:IMG_3687.JPG|250px|left|thumb|Location Building 314, Prep Room 01]]<br />
 
 
<br clear="all" />
<br clear="all" /> -->
 
 
==Sonicators ==
==Sonicators ==