Line 42: Line 42:
[[file:C03991.01 072.jpg|150px|frameless ]]
[[file:C03991.01 072.jpg|150px|frameless ]]
[[file:C03991.01 073.jpg|150px|frameless ]]
[[file:C03991.01 073.jpg|150px|frameless ]]
|-
| 2/5-2016
| 4" Travka20 Wafer
| 20 % Si
| 3 minute TDESC clean
| PrA-0, 80 cycles or 14:40 minutes
| C03991.04
|
[[file:C03991.04 125.jpg|150px|frameless ]]
[[file:C03991.04 126.jpg|150px|frameless ]]
[[file:C03991.04 127.jpg|150px|frameless ]]
[[file:C03991.04 128.jpg|150px|frameless ]]
[[file:C03991.04 129.jpg|150px|frameless ]]
[[file:C03991.04 130.jpg|150px|frameless ]]
[[file:C03991.04 131.jpg|150px|frameless ]]
[[file:C03991.04 132.jpg|150px|frameless ]]
[[file:C03991.04 133.jpg|150px|frameless ]]
[[file:C03991.04 134.jpg|150px|frameless ]]
[[file:C03991.04 135.jpg|150px|frameless ]]
[[file:C03991.04 136.jpg|150px|frameless ]]
[[file:C03991.04 120.jpg|150px|frameless ]]
[[file:C03991.04 121.jpg|150px|frameless ]]
[[file:C03991.04 122.jpg|150px|frameless ]]
[[file:C03991.04 123.jpg|150px|frameless ]]
[[file:C03991.04 124.jpg|150px|frameless ]]
|-
| 3/6-2016
| 4" Travka20 Wafer
| 20 % Si
| 3 minute TDESC clean
| PrA-0, 80 cycles or 14:40 minutes
| C04047.01
|


|-
|-
|}
|}

Revision as of 15:23, 15 June 2016


Process runs
Date Substrate Information Process Information SEM Images
Wafer info Exposed area Conditioning Recipe Wafer ID
2/5-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-0, 80 cycles or 14:40 minutes C03991.01

2/5-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-0, 80 cycles or 14:40 minutes C03991.04

3/6-2016 4" Travka20 Wafer 20 % Si 3 minute TDESC clean PrA-0, 80 cycles or 14:40 minutes C04047.01