Specific Process Knowledge/Etch/Etching of Bulk Glass: Difference between revisions

Fj (talk | contribs)
No edit summary
Fj (talk | contribs)
No edit summary
Line 1: Line 1:
At Danchip, we have two types of bulk glass substrates: Borosilicate glass (Borofloat 33 (like pyrex)) and fused silicate glass which in cleanliness is similar to quartz. Both types are etched wet in a special set-up placed in a fumehood using a strong HF-solution (isotropic etch).
At Danchip, we have two types of bulk glass substrates: Borosilicate glass (Borofloat 33 (like pyrex)) and fused silicate glass which in cleanliness is similar to quartz. Both types are etched wet in a special set-up placed in a fumehood using a strong HF-solution (isotropic etch).
The set-up consists of a 5 l plasic beaker placed on a stirring plate (magnetic stirring) and a special horizontal wafer holder. Normally a 40% pre-mixed HF solution is used.


Masking materials and pre-treatment of the glass surface prior to the deposition of the masking material is a special concern in particular for deep etchings (> 10µm).   
Masking materials and pre-treatment of the glass surface prior to the deposition of the masking material is a special concern in particular for deep etchings (> 10µm).   


Due to the high cleanliness fused silica is allowed access to basically all machines meaning that e.g. LPCVD silicon can be deposited as masking material. This is an excellent mask even for quite deep etchings   
Due to the high cleanliness fused silica is allowed access to basically all machines meaning that e.g. LPCVD silicon can be deposited as masking material. This is an excellent mask even for quite deep etchings.  
40% HF 3µm/min
40% HF 3µm/min
Beaker
Beaker