The effects of [[Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange|changing of the showerhead in December 2014]] was investigated. Patterned wafers were processed before and after and the profile of the etched features were inspectede in SEM.
The effects of [[Specific Process Knowledge/Etch/DRIE-Pegasus/showerheadchange|changing of the showerhead in December 2014]] was investigated. Patterned wafers were processed before and after and the profile of the etched features were inspectede in SEM. Click on the numbers in the 'Runs' column below to see the profiles.
 