Specific Process Knowledge/Thin film deposition/ALD Picosun R200/ALD multilayers: Difference between revisions
Appearance
| Line 29: | Line 29: | ||
Deposition rate: <b>0.089 nm/cycle </b>(@120 <sup>o</sup>C) | Deposition rate: <b>0.089 nm/cycle </b>(@120 <sup>o</sup>C) | ||
This recipe has been developd for fabrication of high quality homogenious optical layers at low temperature. Research related results can be found here:[http://journals.aps.org/prl/abstract/10.1103/PhysRevLett.115.177402 LINK] | This recipe has been developd for fabrication of high quality homogenious optical layers at low temperature. Research related results with this recipe can be found here: [http://journals.aps.org/prl/abstract/10.1103/PhysRevLett.115.177402 LINK] | ||