Specific Process Knowledge/Thin film deposition/ALD Picosun R200/ALD multilayers: Difference between revisions
Appearance
| Line 23: | Line 23: | ||
Recipe: EMA04 | Recipe: EMA04 | ||
Temperature: | Temperature: 120 <sup>o</sup>C | ||
==Al<sub>2</sub>O<sub>3</sub>/TiO<sub>2</sub> multilayers on high aspect ratio structures== | ==Al<sub>2</sub>O<sub>3</sub>/TiO<sub>2</sub> multilayers on high aspect ratio structures== | ||
Revision as of 15:19, 19 May 2016
This page describes non standart recipes including multilayers structures.
Low temperature deposition of Al2O3
Recipe: Al2O3LT
Temperature:80-150 oC
Low temperature deposition of TiO2
Recipe: TiO2LT
Temperature: 80-150 oC
Low temperature grown multilayers on flat surfaces
Recipe: EMA01
Recipe: EMA02
Recipe: EMA03
Recipe: EMA04
Temperature: 120 oC
Al2O3/TiO2 multilayers on high aspect ratio structures
Recipe: Multi T
Temperature: 150C