Jump to content

Specific Process Knowledge/Thin film deposition/ALD Picosun R200/ALD multilayers: Difference between revisions

Eves (talk | contribs)
Eves (talk | contribs)
Line 29: Line 29:
Recipe: Multi T
Recipe: Multi T


Temperature: 120C
Temperature: 150C