| Line 8: | Line 8: | ||
Try and put this as one of the last steps in you process sequence, since you cannot do high temperature steps in DANCHIPS cleanroom with Pyrex wafer. This also includes the plasma systems. | Try and put this as one of the last steps in you process sequence, since you cannot do high temperature steps in DANCHIPS cleanroom with Pyrex wafer. This also includes the plasma systems. | ||