Process recommendations:
Process recommendations:
* a standard process consist of spinning, soft bake, exposure, post bake and development. Please notice that the entire process must be done continuously, meaning that it is not recommendable to spin the resist and then wait until the next day before exposing.
* a standard process consist of spinning, soft bake, exposure, post bake and development. Please notice that the entire process must be done continuously, meaning that it is not recommendable to spin the resist and then wait until the next day before exposing.
* i-line (365nm) radiation is recommended for exposure, therefore use KS or EVG620 aligner, which has i-line filters in the optical system.
* exposure using radiation above 350 nm is recommended. The KS Aligner and Aligner: MA6-2 both have i-line filters, and Aligner: 6inch uses a long-pass filter which reduces the i-line and blocks shorter wavelengths.
* Controlled soft and post bakes are recommended and must be optimized for the specific application, but baseline parameters which can be used as a starting point will be given.
* Controlled soft and post-exposure bakes are recommended and must be optimized for the specific application, but baseline parameters which can be used as a starting point will be given.