Etching of TiO2 using ICP metal has been tested Evgeniy Shkondin @danchip | ===Etching of TiO2 using ICP metal has been tested Evgeniy Shkondin @danchip=== | ||
Recipe used: Ti etch | Recipe used: Ti etch | ||
[[image:TiO2_etch_Evgeniy2.jpg|400px]] | [[image:TiO2_etch_Evgeniy2.jpg|400px]] | ||