Specific Process Knowledge/Pattern Design: Difference between revisions
Appearance
| Line 28: | Line 28: | ||
=== Layout file format=== | === Layout file format=== | ||
* For '''E-beam lithography''' the layout file has to prepared as a GDS file and a v30 file. For details about how to prepare a GDS file and a v30 file for e-beam, please see [[Specific_Process_Knowledge/Lithography/EBeamLithography/FilePreparation#Preparing_a_GDS_file]]. For details about how to make alligned E-beam patterns, please have at look at[[Specific_Process_Knowledge/Lithography/EBeamLithography/JBX9500Manual#Design_of_global_marks_and_chip_marks]] | * For '''E-beam lithography''' the layout file has to prepared as a GDS file and a v30 file. For details about how to prepare a GDS file and a v30 file for e-beam, please see [[Specific_Process_Knowledge/Lithography/EBeamLithography/FilePreparation#Preparing_a_GDS_file|Preparing a GDS file]]. For details about how to make alligned E-beam patterns, please have at look at[[Specific_Process_Knowledge/Lithography/EBeamLithography/JBX9500Manual#Design_of_global_marks_and_chip_marks|Design of global marks and chip marks]] | ||
* For '''laser cutting''' the layout file has to be saved as a DXF file that is uploaded to the equipment computer. For more details concerning pattern design for the laser see [[Specific_Process_Knowledge/Back-end_processing/Mask_making|Mask Making on the Laser Micro Machining Tool]]. | * For '''laser cutting''' the layout file has to be saved as a DXF file that is uploaded to the equipment computer. For more details concerning pattern design for the laser see [[Specific_Process_Knowledge/Back-end_processing/Mask_making|Mask Making on the Laser Micro Machining Tool]]. | ||