Jump to content

Specific Process Knowledge/Etch/KOH Etch: Difference between revisions

Fj (talk | contribs)
Fj (talk | contribs)
Line 108: Line 108:




W<sub>b</sub> = W<sub>o</sub> - 2lcot(54.7<sup>o</sup>) = W<sub>o</sub> - <math>sqrt</math>
W<sub>b</sub> = W<sub>o</sub> - 2lcot(54.7<sup>o</sup>) = W<sub>o</sub> - <math>sqrt(2)</math>l