Jump to content

LabAdviser/314/Preparation 314-307: Difference between revisions

From LabAdviser
Wihu (talk | contribs)
Wihu (talk | contribs)
Line 47: Line 47:
<br clear="all" />
<br clear="all" />


2) Olympus SZ61 stereo Zoom Microscope.
2) TechPrep Allied.
[http://www.olympus-lifescience.com/en/microscopes/stereo/sz61/ Brochure]
[http://www.alliedhightech.com/Equipment/multiprep-polishing-system-8/ Brochure]
[[File:IMG_3673.JPG|left|thumb|Location Building 307, Prep Lab 109]]<br />
[[File:TechPrep.png|200px]|left|thumb|Location Building 307, Prep Lab 109]]<br />
<br clear="all" />
 
3) Struer Labopol -5.
[[File:Labopol5.png|200px]|left|thumb|Location Building 307, Prep Lab 109]]<br />
<br clear="all" />
 
4) Struer Labopol -4.
[[File:Labopol4.png|200px|left|thumb|Location Building 307, Prep Lab 109]]<br />
<br clear="all" />
<br clear="all" />



Revision as of 09:49, 14 January 2016

Feedback to this page: click here


THIS PAGE IS UNDER CONSTRUCTION

Optical Microscopes

1) Olympus BX51 colorview. Operation Manual

Location Building 307, Prep Lab 109



2) Olympus SZ61 stereo Zoom Microscope. Brochure

Location Building 307, Prep Lab 109



3) Leica MZ75 stereo microscope. File:Operation Manual Leica_MZ75.pdf [1]

Location Building 314, Prep Room 01


Ion milling

1) Fischione Low Angle Ion Milling and Polishing System Model 1010. File:Operation Manual Fischione_1010.pdf

Location Building 307, Prep Lab 109

.


2) Fischione NanoMill model 1040. Operation Manual

Location Building 314, Common area


Pumping stations

1) Pumping Cube for single TEM specimen holder.

Location Building 307, Room 111



2) Gatan Turbo Pumping Station model 655. Capacity 4 specimen holders. Brochure

Location Building 314, Common area



Polishing

1) Struers Labopol -25. Brochure

Location Building 307, Prep Lab 109



2) TechPrep Allied. Brochure

Location Building 307, Prep Lab 109



3) Struer Labopol -5.

Location Building 307, Prep Lab 109



4) Struer Labopol -4.

Location Building 307, Prep Lab 109



Saws

Plasma cleaner & Pumping Station

Coaters

Sonicators

Hot plates

Plunger

Microtomes

Critical point dryer

Centrifuge

pH meter