Specific Process Knowledge/Etch/KOH Etch: Difference between revisions
Appearance
| Line 103: | Line 103: | ||
[[Image:KOH_Anisotropy(110).jpg]] | [[Image:KOH_Anisotropy(110).jpg]] | ||
For Si(100), the relation between the width of the bottom of the etched groove (W<sub>b</sub>) and the width of the opening (W<sub>o</sub>) at the wafer surface is given by: | For Si(100), the relation between the width of the bottom of the etched groove (W<sub>b</sub>) and the width of the opening (W<sub>o</sub>) at the wafer surface is given by: | ||