===Definition of structures=== | ===Definition of structures=== | ||
Due to the almost inert (111)-planes it is possible by KOH etching to realize high aspect ratio structures in sigle crytalline silicon. | Due to the almost inert (111)-planes it is possible by KOH etching to realize high aspect ratio structures in sigle crytalline silicon using the (111)-planes as sidewalls. In Si(100) these sidewalls are inclined | ||
[[Image:KOH_Anisotropy.jpg]] | [[Image:KOH_Anisotropy.jpg]] | ||