Specific Process Knowledge/Wafer cleaning/RCA: Difference between revisions
Appearance
| Line 2: | Line 2: | ||
The RCA clean is used for cleaning the wafers before taking them into the furnaces and a few other equipments (check the cross contamination sheet). | The RCA clean is used for cleaning the wafers before taking them into the furnaces and a few other equipments (check the cross contamination sheet). | ||
It | It consists of two solutions: RCA1 and RCA2 plus diluted HF. | ||
The RCA1 contains: H<math>_2</math>O, NH<math>_4</math>OH and H<math>_2</math>O<math>_2</math> (5:1:1). It is used for removed of light organics, particles and metal. <br \> | The RCA1 contains: H<math>_2</math>O, NH<math>_4</math>OH and H<math>_2</math>O<math>_2</math> (5:1:1). It is used for removed of light organics, particles and metal. <br \> | ||