Specific Process Knowledge/Etch/Etching of Gold: Difference between revisions

Kabi (talk | contribs)
Kabi (talk | contribs)
Line 56: Line 56:
*Photoresist
*Photoresist
|
|
*None (only used for stipping Au)
*None (mainly used for stripping Au)
|
|
*Any material that is allowed in the chamber, photoresists included  
*Any material that is allowed in the chamber, photoresists included