Jump to content

Specific Process Knowledge/Characterization/Lifetime scanner MDPmap: Difference between revisions

From LabAdviser
Mdyma (talk | contribs)
Mdyma (talk | contribs)
Line 42: Line 42:
|style="background:LightGrey; color:black"|Detector
|style="background:LightGrey; color:black"|Detector
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Microwave detector
|-
|-
|style="background:LightGrey; color:black"|Laser
|style="background:LightGrey; color:black"|Laser

Revision as of 12:01, 16 November 2015

THIS PAGE IS UNDER CONSTRUCTION

Feedback to this page: click here


Lifetime scanner MPDmap, positioned in cleanroom D-3.


The user manual, control instruction, the user APV and contact information can be found in LabManager:

Lifetime scanner MPDmap info page in LabManager,


Performance information

Equipment performance and process related parameters

Equipment
Purpose
  • Carrier Lifetime
  • Photoconductivity
Location
  • D-3
Performance Resolution
Instrument specifics Detector
  • Microwave detector
Laser
  • 405 nm
    • Power 5 mW to 100 mW
  • 978 nm
    • Power 5 mW to 140 mW
  • 975 nm
    • Power 0.5 W to 4.0 W
  • Spot diameter for all laser 0.5 µm
Substrates Batch size
  • Sample sizs between 5 mm x 5 mm up to 16" or 210 mm x 210 mm
  • Sample thickness 10 µm to 20 mm
Allowed materials
  • Any standard cleanroom materials.