Specific Process Knowledge/Thermal Process/A1 Bor Drive-in furnace: Difference between revisions
Appearance
| Line 2: | Line 2: | ||
[[Image:A1.JPG|thumb|300x300px|A1 Boron drive in furnace: positioned in cleanroom 2]] | [[Image:A1.JPG|thumb|300x300px|A1 Boron drive in furnace: positioned in cleanroom 2]] | ||
A1 Furnace boron drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide | A1 Furnace boron drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide, drive-in of boron after a pre-deposition, oxidation of the boron phase layer. Boron pre-deposition takes place in the A2 Furnace boron pre-dep. It can also be used for drive in of boron which has been ion implanted. | ||
This furnace is the uppermost furnace tube in the furnace A-stack positioned in cleanroom 2. The A-stack together with furnace C1 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart. If you are in doubt, please ask one from the furnace team. | This furnace is the uppermost furnace tube in the furnace A-stack positioned in cleanroom 2. The A-stack together with furnace C1 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart. If you are in doubt, please ask one from the furnace team. | ||
Revision as of 12:33, 27 February 2008
A1 Furnace Boron drive-in
A1 Furnace boron drive-in is a Tempress horizontal furnace for oxidation of silicon wafers, annealing of the grown oxide, drive-in of boron after a pre-deposition, oxidation of the boron phase layer. Boron pre-deposition takes place in the A2 Furnace boron pre-dep. It can also be used for drive in of boron which has been ion implanted.
This furnace is the uppermost furnace tube in the furnace A-stack positioned in cleanroom 2. The A-stack together with furnace C1 are the cleanest of all our furnaces. Please be aware of which substrates are allowed to enter this furnace. Check the cross contamination chart. If you are in doubt, please ask one from the furnace team.
Process knowledge
- Boron drive-in: look at the Dope with Boron page
- Oxidation: look at the Oxidation page
- Annealing: look at the Annealing page
| Purpose | Drive-in of boron, oxidation and annealing | Oxidation:
|
|---|---|---|
| Performance | Film thickness |
|
| Process parameter range | Process Temperature |
|
| . | Process pressure |
|
| . | Gas flows |
|
| Substrates | Batch size |
|
| . | Substrate material allowed |
|