Specific Process Knowledge/Characterization/XPS/Processing/XPSknowledgeview: Difference between revisions
Appearance
No edit summary |
No edit summary |
||
| Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XPS/Processing/XPSknowledgeview click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php?title=Specific_Process_Knowledge/Characterization/XPS/Processing/XPSknowledgeview click here]''' | ||
<!--Checked for updates on 29/7-2018 - ok/jmli --> | |||
= XPS Knowledge View = | = XPS Knowledge View = | ||
Revision as of 10:58, 30 July 2018
Feedback to this page: click here
XPS Knowledge View
The XPS Knowledge View shown here is from Avantage version 5.948.
- Click the knowledge view button in the toolbar to the left in Avantage as shown with a red square.
- A tab pops up in the window. Click on the periodic table as shown to select an element.