Jump to content

Specific Process Knowledge/Wafer cleaning: Difference between revisions

From LabAdviser
BGE (talk | contribs)
BGE (talk | contribs)
Line 1: Line 1:
== Clean with: ==
== Clean with: ==


*[[Cleaning with RCA|RCA]] - ''Two step process to remove organics and metals''
*[[/RCA|RCA]] - ''Two step process to remove organics and metals''
*[[Cleaning with 7-up|7-up]] - ''Fake piranha etch of wafers and masks - removes organics and alkali ions''
*[[/7-up|7-up]] - ''Fake piranha etch of wafers and masks - removes organics and alkali ions''
*[[Cleaning with Piranha|Piranha]] - ''Removes organics and alkali ions''
*[[/Piranha|Piranha]] - ''Removes organics and alkali ions''
*[[Cleaning with BHF|BHF]] - ''Removing native oxide, etching of predep glass etc.''
*[[/cleaning with BHF|BHF]] - ''Removing native oxide, etching of predep glass etc.''
*[[Cleaning with IMEC|IMEC]] - ''Cleaning before fusion bonding''
*[[/IMEC|IMEC]] - ''Cleaning before fusion bonding''
*[[Cleaning with Soap Sonic|Soap Sonic]] - ''Cleaning of "dirty" wafers when entering the cleanroom''
*[[/Cleaning with Soap Sonic|Soap Sonic]] - ''Cleaning of "dirty" wafers when entering the cleanroom''

Revision as of 08:25, 18 October 2007

Clean with:

  • RCA - Two step process to remove organics and metals
  • 7-up - Fake piranha etch of wafers and masks - removes organics and alkali ions
  • Piranha - Removes organics and alkali ions
  • BHF - Removing native oxide, etching of predep glass etc.
  • IMEC - Cleaning before fusion bonding
  • Soap Sonic - Cleaning of "dirty" wafers when entering the cleanroom