| Line 3: | Line 3: | ||
If the film quality for the wet oxide is acceptable then the thickness and the time it takes to grow the oxide often decides if a dry or wet oxidation is chosen. | If the film quality for the wet oxide is acceptable then the thickness and the time it takes to grow the oxide often decides if a dry or wet oxidation is chosen. | ||
*Dry oxide is used from 5nm - 200nm. Can be grown in furnaces:A1,A3,C1,C2,C3. | *Dry oxide is used from 5nm - 200nm. Can be grown in furnaces:A1,A3,C1,C2,C3. | ||
*Wet oxide with | *Wet oxide with O<math>_2</math> and H<math>_2</math> can be grown in furnace:A1,A3. | ||
*Wet oxide with | *Wet oxide with H<math>_2</math>O in a bubbler can be grown in furnaces:C1,C2,C3. | ||
==Comparing the six oxidation furnaces== | ==Comparing the six oxidation furnaces== | ||