Jump to content

Specific Process Knowledge/Characterization/XPS/Processing/Basics/2highres: Difference between revisions

Jmli (talk | contribs)
Jmli (talk | contribs)
Line 110: Line 110:
[[File:XPS-basics19b.jpg|300px]]
[[File:XPS-basics19b.jpg|300px]]


The analysis continues <span>[[Specific_Process_Knowledge/Characterization/XPS/Processing/Basics/3fitting#top|here]]</span>
The result is that we have fitted all levels of the Si2p peak. Since silicon is not the only element in the sample, we need to apply the same procedures to the other core levels. The analysis continues <span>[[Specific_Process_Knowledge/Characterization/XPS/Processing/Basics/3fitting#top|here]]</span>.