Please note that all new materials have to be approved by the Thin Film group (thinfilm@danchip.dtu.dk) before they are allowed in the furnace.  
Please note that all new materials have to be approved by the Thin Film group (thinfilm@danchip.dtu.dk) before they are allowed in the furnace.  


The furnace tube is heated by use on 12 long heaters situated along the furnace tube and two flat heaters situated in the ends of the furnace tube. The this way the temperature will be very uniform everywhere in the furnace tube. The heating can be done very fast, up to 30 <sup>o</sup>C/min. For atmospheric pressure processes the maximum temperature is 1100 <sup>o</sup>C, and for vacuum processes the maximum temperature is 1050 <sup>o</sup>C. Cooling is done (rather slowly) by use of cooling fans.
The furnace tube is heated by use on 12 long heaters situated along the furnace tube and combined in three groups (top, bottom left and bottom right) and two flat heaters situated in the ends of the furnace tube. The this way the temperature will be very uniform everywhere in the furnace tube. The heating can be done very fast, up to 30 <sup>o</sup>C/min. For atmospheric pressure processes the maximum temperature is 1100 <sup>o</sup>C, and for vacuum processes the maximum temperature is 1050 <sup>o</sup>C.  
 
The furnace body surrounding the furnace tube consists of a top and bottom half-shell. To cool down the furnace, the top half shelf can be lifted up, and cooling fans will then flow air from the surroundings around the furnace tube to cool it down. However, for safety reasons, the cooling fans will not the activated when there is hydrogen in the furnace, and cooling will then be very slow. Furthermore t
 
It is not possible to open the furnace when the temperature is above 800 <sup>o</sup>C.


For resist pyrolysis, samples with different resist layers are heated up to maximum 1100 <sup>o</sup>C in a nitrogen atmosphere. At high temperatures carbon is formed by pyrolysis of the resist. In this way conductive structures can be made from a resist patterned sample. If oxygen from the air or from outgassing of the resist is present in the furnace, the resist layer will be removed, thus it is important to evacuate the furnace and flush it with nitrogen, before a high temperature for resist pyrolysis is obtained. Pyrolysis of a large amount of resist may also be a problem due to resist outgassing.  
For resist pyrolysis, samples with different resist layers are heated up to maximum 1100 <sup>o</sup>C in a nitrogen atmosphere. At high temperatures carbon is formed by pyrolysis of the resist. In this way conductive structures can be made from a resist patterned sample. If oxygen from the air or from outgassing of the resist is present in the furnace, the resist layer will be removed, thus it is important to evacuate the furnace and flush it with nitrogen, before a high temperature for resist pyrolysis is obtained. Pyrolysis of a large amount of resist may also be a problem due to resist outgassing.