Jump to content

Specific Process Knowledge/Characterization/XPS/Processing/Basics/2highres: Difference between revisions

From LabAdviser
Jmli (talk | contribs)
Jmli (talk | contribs)
Line 20: Line 20:
[[File:XPS-basics12.jpg|700px]]
[[File:XPS-basics12.jpg|700px]]


A window with a suggestion to a peak will pop up. In the spectrum the location and width of the peak is shown
== Peak fitting ==
<span style="font-size: 90%; text-align: right;">[[Specific_Process_Knowledge/Characterization/XPS/Processing/Basics/2highres#top|Go to top of this page]]</span>


<span style="font-size: 90%; text-align: right;">[[Specific_Process_Knowledge/Characterization/XPS/Processing/Basics/2highres#top|Go to top of this page]]</span>
A window labelled 'Peak Fitting' with a suggestion to a peak (see red square) will pop up. Usually the peak is correctly identified, in this case it's a Si2p doublet. The window has two tabs - first we will set up the 'Add Fitted Peak'.
 
[[File:XPS-basics13.jpg|700px]]
 
In the spectrum the location and width of the peak are shown with bars (see blue square) - you can modify the location and the width using the mouse. Here we start out with the bulk peak as shown. Once this peak is fixed we will add the Si2p oxide peak.
 
The green square holds the information on how to correct for the background. In this case we will use the 'Shirley' background with default settings.

Revision as of 09:26, 9 September 2015

Selecting high resolution spectra for peak fitting

The analysis of the data from here is continued. Open a new data grid and drag the four sets of spectra into each quadrant as seen below.

Scroll up or down through the levels of one spectrum by using the scroll button (either etch level or etch time). If several spectra are selected simultaneously by pressing SHIFT or CTRL while clicking on the spectra in the four quadrant view, you watch the evolution of the spectra together.

To analyze a single spectrum, select and maximize it. Before adding peaks to the spectrum, it is a good idea consider what you know about the sample. Here, we know that the sample has ALD deposited layers of ZnO and CuZn on top of a silicon substrate. One would therefore expect to see bulk silicon provided we sputter deep enough and oxidized silicon from the native oxide. Therefore, scroll to a level where, preferably, both the oxidized Si2p and the bulk silicon Si2p are visible. In this case, it is level 35.

Click the 'Peak Fit' button in the top to enable peak fitting on all levels.

Peak fitting

Go to top of this page

A window labelled 'Peak Fitting' with a suggestion to a peak (see red square) will pop up. Usually the peak is correctly identified, in this case it's a Si2p doublet. The window has two tabs - first we will set up the 'Add Fitted Peak'.

In the spectrum the location and width of the peak are shown with bars (see blue square) - you can modify the location and the width using the mouse. Here we start out with the bulk peak as shown. Once this peak is fixed we will add the Si2p oxide peak.

The green square holds the information on how to correct for the background. In this case we will use the 'Shirley' background with default settings.