XPS data processing guide
This section shows all actions performed with Avantage during an analysis of a sample
Open data and save the processing document
- Locate the .VGX file in the experiment data tree.
- Either open the experiment by selecting 'Open Experiment' in Avantage, or
- Double click on the .VGX file.