The XPS Knowledge View described here is from Avantage version 5.948.
The XPS Knowledge View described here is from Avantage version 5.948.
[[File:XPS-knowledgeview2.jpg|400px]]
 
[[File:XPS-knowledgeview2.jpg|700px]]


# Click the knowledge view button in the toolbar to the left in Avantage as shown with a red square.
# Click the knowledge view button in the toolbar to the left in Avantage as shown with a red square.
# A tab pops up in the window. Click on the periodic table as shown to select an element.
# A tab pops up in the window. Click on the periodic table as shown to select an element.

Revision as of 11:37, 8 September 2015

XPS Knowledge View

The XPS Knowledge View described here is from Avantage version 5.948.

  1. Click the knowledge view button in the toolbar to the left in Avantage as shown with a red square.
  2. A tab pops up in the window. Click on the periodic table as shown to select an element.