Specific Process Knowledge/Thin film deposition/Deposition of Alumina: Difference between revisions
Appearance
Created page with "'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thi..." |
No edit summary |
||
| Line 1: | Line 1: | ||
=<span style="background:#FF2800">THIS PAGE IS UNDER CONSTRUCTION</span>[[image:Under_construction.png|200px]]= | |||
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/ALD_Picosun_R200/Standard_recipes_on_the_ALD_tool click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/ALD_Picosun_R200/Standard_recipes_on_the_ALD_tool click here]''' | ||
Revision as of 10:53, 7 September 2015
THIS PAGE IS UNDER CONSTRUCTION
Feedback to this page: click here
Feedback to this page: click here
Deposition of Titanium Oxide
Titanium oxide can be deposited either by a sputter technique or by use of ALD (atomic layer deposition). At the moment the only system where we have a target for Titanium oxide is IBE/IBSD Ionfab300. The target is Ti. During the sputter deposition oxygen is added to the chamber resulting in Titanium oxide on the sample.
Comparison of the methods for deposition of Titanium Oxide
| Sputter technique using IBE/IBSD Ionfab300 | Sputter System Lesker | III-V Dielectric evaporator | ALD Picosun 200 | |
|---|---|---|---|---|
| Generel description |
|
|
|
|
| Stoichiometry |
|
|
|
|
| Film Thickness |
|
|
|
|
| Deposition rate |
|
|
|
|
| Step coverage |
|
|
|
|
| Process Temperature |
|
|
|
|
| More info on TiO2 |
|
|
||
| Substrate size |
|
|
|
|
| Allowed materials |
|
|
|